Skip to main content
. 2020 Jan 10;13(2):329. doi: 10.3390/ma13020329

Figure 10.

Figure 10

X-ray diffraction patterns of loratadine loaded into the alginate-based aerogel: (a) 24.32, (b) 26.92, (c) 30.55 wt %.