Skip to main content
. 2019 Oct 9;21:91–102. doi: 10.1016/j.jare.2019.10.002

Fig. 3.

Fig. 3

The influence of DA soaking concentration on composite fibers. SEM micrograph of composite fibers at DA concentration of (a) 0.0 g·L−1, (b) 0.5 g·L−1 and (c) 1.0 g·L−1. Ag distribution on composite fibers at DA concentration of (d) 0.0 g·L−1, (e) 0.5 g·L−1 and (f) 1.0 g·L−1. EDS analysis of composite fibers at DA concentration of (g) 0.0 g·L−1, (h) 0.5 g·L−1 and (i) 1.0 g·L−1. (j) FTIR spectrum of composite fibers with DA concentration of 0.5 g·L−1.