Figure 1.
(A) The schematic of the packaging using electrospinning method. (B–I) SEM images in two magnitudes (×0.5 k (top), ×1.5 k (bottom)) of nanofibers with %1, 3% and 5% of tea tree (TT) oil (the red and white arrow indicates the nanofiber with diameter of 1 µm and 200 nm, respectively). (J–M) Histogram of diameter of nanofibers with 1%, 3% and 5% of TT oil. (N) Stress–strain curve of nanofibers with different concentrations of TT oil.