Figure 13

(a) Top-view scanning electron micrographs of TNT arrays prepared by anodizing Ti in a mixed ethylene glycol/NH4F and water solution under applied voltages of 5, 15 and 20 V for 5 h. Reproduced with permission from [225]. Copyright IOP Publishing, 2014. (b) Cross-sectional SEM image (inset) and top view of TNTs fabricated by anodizing Ti in a mixed ethylene glycol/NH4F and water solution at 30 V for 1 h. Reproduced with permission from [223]. Copyright MDPI, 2019.