Skip to main content
. 2019 Dec 19;12(1):15. doi: 10.3390/polym12010015

Figure 5.

Figure 5

Figure 5

Comparison of SEM micrographs of: neat PET textile (a) and PUD/PET (b), at the same magnification (×250). SEM micrographs of PUD/PET surface at a higher magnification of ×500 (c) and of ×1000 (d). Dashed arrows are used in the figures to highlight the presence of polyurethane within the fabric weaving.