Flexural strength of cement mortars incorporating GO/GR hybrid.

GO:GR Flexural Strength (MPa) Increment (%)
3 d 7 d 28 d 3 d 7 d 28 d
0:0 6.12 8.48 9.60
1:0 6.80 8.72 10.20 11.11 2.83 6.25
3:1 7.52 9.62 11.29 22.88 13.44 17.60
1:1 7.66 10.06 12.55 25.16 18.63 30.73
1:3 7.46 9.88 11.82 21.90 16.51 23.13
0:1 6.77 8.70 11.73 10.62 2.59 22.19