Skip to main content
. 2019 Dec 25;12(1):36. doi: 10.3390/polym12010036

Figure 7.

Figure 7

Time dependence on (a) hydrodynamic radius (Rh) and (b) light-scattering intensity (LSI) for PEG54-P(AA/VE6/γTCP29)140 at Cp = 0.10 g/L at 25 °C in acetate buffer of pH 5.2 (○) and in PBS buffer of pH 7.4 (△).