TGA and DTG data of EP composites.

Samples T5% (°C) Tmax (°C) Vmax (%/min) R-Mass (%)
Pure EP 356.3 371.7 15.87 17.99
g-C3N4-EP 356.3 371.7 13.85 18.83
g-C3N4/PAZn-EP 346.7 361.2 11.99 23.21