Skip to main content
. 2020 Jan 20;25(2):428. doi: 10.3390/molecules25020428

Figure 8.

Figure 8

11B/31P 2D maps obtained on (a) sodium borophosphate glass at 9.4 T with the CP-HETCOR sequence, (b) lithium borophosphate glass at 9.4 T with the D-HMQC and (c) lithium borophosphate glass at 18.8 T with the J-HMQC NMR techniques [19,26,33]. Reprinted with permission from Elsevier and RSC.