Table 2.

UV light‐induced ATRP of MMA using CDs under different experimental conditions (t=exposure time, L=TPMA; tris(2‐pyridylmethyl)amine)[a]

Run

[MMA]/[RX]/[CD]/[CuBr2]/[L]

t

[h]

x [b]

[%]

M n [c]

[g mol−1]

Đ [c]

1

300:1:0.3:0.03:0.135

0.5

5.5

23 000

1.3

2

300:1:0.6:0.03:0.135

2.5

30

6000

1.2

3

300:1:0:0.03:0.135

1

4

300:1:0.3:0:0.135

1

<1

40 0000

2.4

5

300:1:0.15:0.03:0.135

4

[a] Polymerization experiments were performed at 405 nm at room temperature. [b] Conversion (x) determined gravimetrically. [c] Determined by gel permeation chromatography using PMMA standards.