Table 1.

Means and standard deviations for push-out bond strength values (MPa) of different calcium silicate cements with respect to intracanal medicaments

Intracanal Medicaments P-value
Control Ca(OH)2 mTAP
MTA 88.14 ± 33.43a,A 58.81 ± 16.28b,A 50.76 ± 9.65b,A 0.00
BC fast set putty 78.18 ± 11.65a,A 69.19 ± 37.47a,A 70.85 ± 23.34a,B 0.63
P-value 0.31 0.35 0.01

MTA, ProRoot mineral trioxide aggregate; BC fast set putty, TotalFill Root Repair Material fast set putty; Ca(OH)2, Calcium hydroxide; mTAP, modified triple antibiotic paste. Different superscripted lowercase letters indicate statistically significant differences in dislodgement resistance between the control, Ca(OH)2, and mTAP groups within each material (p < .05). Different superscripted uppercase letters indicate statistically significant differences in dislodgement resistance between MTA and BC fast set putty within each intracanal medicament group (p < .05)