(a) TEM micrographs of Zn0.5Fe2.5O4 NPs. (b) High-resolution TEM image of Zn0.5Fe2.5O4 NPs. (c) TEM micrographs of silica-coated Zn0.5Fe2.5O4 NPs. (d) XRD pattern of Zn0.5Fe2.5O4/SiO2 NPs, the main reflections are (220), (311), (222), (400), (511), (440) according to PDF#86-0509-jade. (e) Hysteresis loop for 22 nm Zn0.5Fe2.5O4/SiO2 NPs recorded at room temperature pointing to the superparamagnetic characteristics of NPs. (f) Field dependence of SAR for Zn0.5Fe2.5O4/SiO2 NPs. (g) Heating curves of aqueous solutions of 22 nm Zn0.5Fe2.5O4/SiO2 NPs (1 mg NPs ml−1).