Table 4.
Temperature measured in the centre of specimens at the adhesive layer in 5 °C water bath at different dwell times (n = 25).
| Specimen designation |
|||
|---|---|---|---|
| e | f | g | |
| Specimen size | 10 mm Ø×10 mm composite cylinder on tooth | 10 mm Ø×10 mm composite cylinder on tooth, mounted in resin | 2.38 mm Ø×4 mm composite cylinder on tooth, mounted in resin |
| Dwell time (s) | |||
| 20 | 17.6 ± 0.35 °C | 22.4 ± 1.40 °C | 7.6 ± 0.13 °C |
| 30 | 13.0 ± 0.15 °C | 18.5 ± 0.19 °C | 7.0 ± 0.08 °C |
| 40 | 8.7 ± 0.31 °C | 16.0 ± 0.56 °C | 6.2 ± 0.15 °C |
| 50 | 7.4 ± 0.27 °C | 14.3 ± 0.25 °C | 6.1 ± 0.19 °C |
| 60 | 6.3 ± 0.09 °C | 12.9 ± 0.17 °C | 6.0 ± 0.14 °C |