Skip to main content
. 2020 Jan 29;7(1):16–24. doi: 10.1080/26415275.2019.1709470

Table 5.

Temperature measured in the centre of specimens at the adhesive layer in 55 °C water bath at different dwell times (n = 25).

  Specimen designation
  e f g
Specimen size 10 mm Ø×10 mm composite cylinder on tooth 10 mm Ø×10 mm composite cylinder on tooth, mounted in resin 2.38 mm Ø×4 mm composite cylinder on tooth, mounted in resin
Dwell time (s)      
20 42.2 ± 0.45 °C 37.8 ± 1.00 °C 53.2 ± 0.15 °C
30 46.9 ± 0.20 °C 41.6 ± 0.17 °C 53.9 ± 0.14 °C
40 50.2 ± 0.16 °C 43.7 ± 0.66 °C 54.2 ± 0.28 °C
50 52.4 ± 0.30 °C 45.8 ± 0.19 °C 54.4 ± 0.20 °C
60 53.8 ± 0.22 °C 46.9 ± 0.12 °C 54.7 ± 0.15 °C