Skip to main content
. 2020 Jan 29;7(1):16–24. doi: 10.1080/26415275.2019.1709470

Table 6.

Repair micro-tensile bond strength of test specimens stored in water for 3 months and tested after thermal cycling and without thermal cycling.

3 months in water + thermal cycling
(n = 24 in each group)
3 months in water (control)
(n = 8 in each group)
outer specimens inner specimens outer specimens inner specimens
37.8 ± 8.8 MPaA,B,C 55.5 ± 8.5 MPaA 58.3 ± 4.2 MPaB 59.1 ± 6.4 MPaC

Groups with same upper-case letters are statistically significant different (p < .05).