Antifouling loop-forming triblock copolymers. (A) structure of loop and linear polymers and representation of their use for coating a surface. (B) top: QCM-D traces showing changes in frequency and dissipation upon the absorption of BSA on surfaces uncoated or coated with loop or lineal PEG, and bottom: quantification of protein adsorption on the same surfaces (ng/cm). Reprinted (adapted) with permission from reference [51]. Copyright (2015) Royal Chemical Society.