Skip to main content
. 2020 Jan 27;17(3):788. doi: 10.3390/ijerph17030788

Figure 4.

Figure 4

(a) Comparison of adsorption capacity among chitosan, chitosan-kenaf biochar, chitosan-BiFeO3, CKB and kenaf biochar: C0Cr(VI) = 50mg/L, W = 0.2 g, T = 30 °C, t = 4 h, pH = 2, (b) Effect of solution pH on Cr(VI) adsorption onto CKB: C0Cr(VI) = 50 mg/L, W = 0.2 g, T = 30 °C, t = 4 h, (c) Effect of Ca2+, NO3, PO43−, and SO42− on Cr(VI) adsorption onto CKB: C0Cr(VI) = 50 mg/L, W = 0.2 g, T = 30 °C, t = 4 h, pH = 2.