Table 6.
Shares of different types of carbon, nitrogen, and oxygen atoms in the cross-linked graphene oxide powder obtained by the deconvolution of the C1s band.
Atomic Concentration (%) 1s Binding Energy |
C-S1GO | C-S2GO | C-S3GO | C-M1GO | C-M2GO | C-L2GO |
---|---|---|---|---|---|---|
C (285 eV) | 58.57 | 57.36 | 40.29 | 61.27 | 54.64 | 60.52 |
C (286 eV) | 17.52 | 18.97 | 19.65 | 16.25 | 19.05 | 17.20 |
C (290 eV) | 16.68 | 14.40 | 21.62 | 14.55 | 15.55 | 15.22 |
N (400 eV) | 0.64 | 1.58 | 2.58 | 0.52 | 1.58 | 0.42 |
N (404 eV) | 0.56 | - | - | 0.60 | - | 0.34 |
O (532 eV) | - | 7.69 | - | 3.61 | 9.18 | 3.14 |
O (533 eV) | 5.13 | - | 9.81 | 3.20 | - | 3.15 |
O (537 eV) | 0.91 | - | - | - | - | - |
O (539 eV) | - | - | 6.04 | - | - | - |