Mixture ratio of GO concrete (kg/m3).

Number Cement Fly Ash Silica Fume Machine-Made Sand Coarse Aggregate GO Water Polycarboxylate Superplasticizer
PC50 370 70 28 723 1085 0 164 6.08
GOC50-1 370 70 28 723 1085 0.074 164 6.08
GOC50-2 370 70 28 723 1085 0.185 164 6.08
GOC50-3 370 70 28 723 1085 0.296 164 6.08