Skip to main content
. 2020 Feb 5;13(3):730. doi: 10.3390/ma13030730

Figure 2.

Figure 2

Dependence of the electrical resistivity of the lines from silver nano-ink on the temperature of the substrate heating (a); SEM image of a line dried at 100 °C (b) and sintered at 400 °C (c), respectively. The formation of the lines was carried out at Ts = 25 °C, N = 1 layer, FR = 5 and Vs = 100 mm/min.