Skip to main content
. 2020 Feb 5;13(3):730. doi: 10.3390/ma13030730

Figure 3.

Figure 3

Temperature dependence of the resistance of dried and sintered lines after heat treatment for 60 minutes formed at temperatures of 100 °C (a) and 400 °C (b), respectively. The formation of this lines was carried out at Ts = 25 °C, N = 1 layer, FR=5 and Vs = 100 mm/min.