Skip to main content
. 2019 Dec 13;5(7):3144–3150. doi: 10.1021/acsomega.9b02524

Figure 3.

Figure 3

Mechanical strength test by repetitive 3M Scotch tape peeling. (A) ZnO nanostructures without the tape peeling test. (B) ZnO nanostructures after 10 times tape peeling tests.