. 2020 Feb 27;10:3627. doi: 10.1038/s41598-020-60458-9

Figure 6.

Figure 6

DSC crystallization curves of PDLA-PEG-PDLA triblock copolymers with different PEG segments at a cooling rate of 10 °C/min: (A) PEG with different molecular weights is 2000, 4000, 6000, and 8000; (B) PEG and D-LA/PEG with various ratios of 1/1, 2/1, and 3/1.