Skip to main content
. 2020 Feb 25;7(1):50–60. doi: 10.1080/26415275.2020.1728277

Table 2.

Comparisons of the marginal gaps for the different material groups and bonding protocols.

  Total-etch
Self-etch
Variables Mean Ceramill COMP Cerasmart p-Value  Mean Ceramill COMP Cerasmart p-Value 
Before                
 Mean 46.6 45.4 47.7 0.3 48.2 47.9 48.4 .7
 SD 6.4 5.7 6.9 7.1 6.6 7.8
After                
 Mean 43.4 40.8 45.9 .002*** 45.7 45.4 46.1 .06
 SD 5.5 6.1 3.2 4.6 5.7 3.2
p-Value .004* .002** 0.3   .04*a 0.2 0.08  

*Significant difference between the two bonding protocols. **Significant difference between each bonding protocol before and after aging for each material approach. ***Significant difference between the two endocrown materials.