Table 3.
Comparisons of the load required to fracture the endocrown with respect to the material used and different bonding protocols.
| Variables | Mean load required to fracture |
p-Value | |
|---|---|---|---|
| Mean | SD | ||
| Material cementation approach | |||
| Ceramill COMP | 2420 | 1027 | .6 |
| Cerasmart | 2220 | 515 | |
| Bonding protocols | |||
| Total-etch | 2238 | 750 | .6 |
| Self-etch | 2402 | 875 | |
| Bonding protocolsin Ceramill COMP cementation | |||
| Total-etch | 2532 | 930 | .7 |
| Self-etch | 2308 | 1194 | |
| Bonding protocolsin Cerasmart cementation | |||
| Total-etch | 1944 | 406 | .06 |
| Self-etch | 2496 | 487 | |