SEM images of MoSx~2+δ/Mo films obtained on the (a) Si, (b) SiO2, and (c) glassy carbon (GC) substrates by on-axis PLD in Ar at a pressure of 8 Pa. The deposition times were (a) 4 min, (b) 64 min, and (c) 64 min. (b) The top inset shows a cross-sectional image of the film.