Skip to main content
. 2020 Jan 24;10(2):201. doi: 10.3390/nano10020201

Figure 12.

Figure 12

(a) Polarization curves. (b) Anodic cyclic voltammograms. (c) TOF dependence on voltage for the MoSx~2+δ/Mo catalysts obtained on the GC substrate by on-axis PLD in Ar at 8 Pa for different deposition times.