Surface porosity evaluation of PLA (a) and PLA-10CaSi-10DCPD (b) scaffolds on one random area at 500× and 1000× magnifications. Mineral doped formulation revealed a more compact surface, with a lower number of porosities when compared to pure PLA formulation.