A comparison of the mechanical properties of the prepared blends from tensile and impact resistance measurements for the “as-molded” samples. (A) Tensile modulus and strength. (B) Elongation at break and impact strength. Results are grouped into PLA-, POM-, and POM/PLA-based samples modified using the ethylene/butyl acrylate/glycidyl methacrylate terpolymer (E/BA/GMA) elastomer (EBA) impact modifier and epoxy-functional styrene acrylic copolymer (ESA) chain extender (CE).