TGA data of FK/PVA/PEO composite nanofibers with different AgNPs amounts.

Sample (%) T10 (°C) Tmax1 (°C) Tmax2 (°C)
0%-AgNPs 240 255 406
0.6%-AgNPs 245 262 408
1.2%-AgNPs 250 264 409
1.8%-AgNPs 253 267 410
2.4%-AgNPs 254 272 411
3%-AgNPs 256 273 413

Note: T10 is the temperature of 10% mass loss. Tmax1 and Tmax2 are the temperature with the fastest mass loss in the second and third weight loss stage, respectively.