Tensile strength (TS) and elongation at break (EAB) of FK/PVA/PEO composite nanofibers with different AgNPs amounts.

Samples TS (MPa) EAB (%)
0%-AgNPs 2.62 ± 0.51 42.75 ± 0.25
0.6%-AgNPs 4.30 ± 0.64 31.25 ± 5.30
1.2%-AgNPs 5.52 ± 0.71 51.50 ± 9.19
1.8%-AgNPs 4.83 ± 1.23 30.50 ± 5.57
2.4%-AgNPs 2.60 ± 0.51 20.93 ± 10.42
3.0%-AgNPs 2.38 ± 0.57 12.5 ± 3.27