Skip to main content
. 2020 Feb 11;12(2):406. doi: 10.3390/polym12020406

Figure 7.

Figure 7

Typical galvanostatic charge–discharge potential profiles vs. Li/Li+ for the 10th, 20th, 30th, 40th, and 50th cycle against the capacity of the pre-lithiated CNT electrode for 15 min at 1 C rate (a), rate capabilities of the pre-lithiated CNT electrode for 15 min at 1 C rate (b) and multiple C-rates (c).