Skip to main content
. 2020 Feb 17;12(2):461. doi: 10.3390/polym12020461

Figure 4.

Figure 4

SEM micrographs of bonding interface of the experimental adhesives when SE was applied. Magnification of 500× (E,G) and 2000× (F) were used. E and F—AE1 with 10.4 µm of HL thickness; (G)—AE2. RC—resin composite; D—dentin; HL—hybrid layer; RT—resin tags; AF—adhesive failure.