Figure 2.

Figure 2

Flexural and compressive strengths of the samples (28 days curing). The label EPS (expanded polystyrene) represents EPS 2, EPS3, and EPS4. White squares represent the compressive strengths, while black squares represent flexural strengths. In the inset: inner porosity of an EPS bead (SEM image).