Skip to main content
. 2020 Feb 19;13(4):928. doi: 10.3390/ma13040928

Figure 6.

Figure 6

(a) Strain path evolution along a section perpendicular to the crack of a TS specimen for different stages through the Nakajima test. Measured major strains obtained by the DIC system for several stages: (b) No deformation; (c) onset of necking; (d,e) steadily neck propagation; (f) ceasing of neck propagation and (g) fracture.