Skip to main content
. 2020 Feb 19;13(4):928. doi: 10.3390/ma13040928

Figure 8.

Figure 8

Fractography of a PT Nakajima specimen with 1 mm of thickness. Magnification of: (a) The fracture zone and (b) the transition zone.