The electrochemical parameters derived from Nyquist diagrams of an iron electrode in a 1M HCl solution without and with different concentration of the Galactomannan.

Concentrations (g/l) Re (Ω.cm2) Rt (Ω.cm2) CPE (mF.n−1) α Cdl (mF) E (%)
Blank 0.5 ± 0.1 68.5 ± 0.2 0.368 ± 0.002 0.70 ± 0.02 152.5 ± 0.2
0.25 1.3 ± 0.1 341.7 ± 0.2 0.245 ± 0.003 0.71 ± 0.02 0.917 ± 0.003 80 ± 0.1
0.50 1.3 ± 0.1 360.1 ± 0.2 0.210 ± 0.0015 0.73 ± 0.01 0.802 ± 0.001 81 ± 0.2
0.75 1.4 ± 0.1 446.6 ± 0.1 0.141 ± 0.004 0.79 ± 0.02 0.672 ± 0.004 84 ± 0.1
1.00 1.4 ± 0.1 490.4 ± 0.2 0.131 ± 0.005 0.78 ± 0.01 0.625 ± 0.005 86 ± 0.2