Skip to main content
. 2020 Mar 20;10:5111. doi: 10.1038/s41598-020-61933-z

Figure 2.

Figure 2

SEM images of poly(ether)urethane layer after peeling of electrospun fibrin layer (O.M. 100× and 300×).