Tensile strength, Young’s modulus, and elongation at break of SA-GO30L-4000 nanocomposite series and pure SA matrix.

Sample Tensile Strength (MPa) Young’s Modulus (GPa) Elongation at Break (%)
SA 101.4 ± 4.8 3.0 ± 0.1 12.8 ± 3.9
SA-GO30L-4000-1% 104.5 ± 9.1 3.3 ± 0.3 10.2 ± 0.9
SA-GO30L-4000-4% 111.9 ± 15.1 3.2 ± 0.5 14.6 ± 2.9
SA-GO30L-4000-6% 108.3 ± 8.9 3.6 ± 0.3 11.3 ± 1.6
SA-GO30L-4000-8% 119.1 ± 6.2 3.7 ± 0.3 9.0 ± 3.0