Skip to main content
. 2020 Mar 3;13(5):1120. doi: 10.3390/ma13051120

Figure 3.

Figure 3

Severe formation of microcracks in the matrix (marked with red arrows) of a high strength LC due to water absorption of fine and coarse LWA (Courtesy: Andrea Kustermann).