Table 2.
LCR-TMP specific energy targets and wt% of HC-TMP and microfibres used in the composite samples
| Specific energy target (kWh/t) | LCR-TMP | HC + TMPMF (1567) | HC + TMPMF (2242) | HC + KMF (2430) | ||||
|---|---|---|---|---|---|---|---|---|
| LCR-TMP | HC-TMP | TMPMF (1567) | HC-TMP | TMPMF (2242) | HC-TMP | KMF (2430) | HC-TMP | |
| (wt%) | (wt%) | (wt%) | (wt%) | (wt%) | (wt%) | (wt%) | (wt%) | |
| 0 | 0 | 100a | – | – | – | – | – | – |
| 113 | 100 | 0 | 7 | 93 | 5 | 95 | 5 | 95 |
| 228 | 100 | 0 | – | – | 10 | 90 | – | – |
| 315 | 100 | 0 | 20 | 80 | 14 | 86 | 13 | 87 |
| 387 | 100 | 0 | – | – | 17 | 83 | – | – |
| 493 | 100 | 0 | 31 | 69 | 22 | 78 | 20 | 80 |
aHC-TMP sample (primary pulp)