Table 3.
Biomechanical data of rabbits implanted with polypropylene and ACTM after 24 weeks.
Tensile stress (MPa) | Tensile strain (%) | |||
---|---|---|---|---|
Polypropylene | ACTM | Polypropylene | ACTM | |
14.05 | 11.22 | 43.32 | 67.22 | |
12.65 | 10.65 | 50.25 | 60.34 | |
12.88 | 11.05 | 46.98 | 66.22 | |
15.02 | 12.08 | 47.44 | 66.56 | |
14.76 | 12.21 | 49.06 | 59.02 | |
14.00 | 10.98 | 48.10 | 58.84 | |
13.52 | 11.14 | 50.80 | 70.05 | |
15.14 | 12.32 | 47.96 | 71.14 | |
15.04 | 12.20 | 48.23 | 68.43 | |
12.98 | 12.34 | 48.21 | 65.23 | |
12.90 | 11.76 | 41.22 | 55.92 | |
13.45 | 11.91 | 47.08 | 57.28 | |
14.22 | 11.02 | 49.19 | 59.11 | |
14.43 | 11.30 | 58.00 | 58.48 | |
15.28 | 12.01 | 43.09 | 63.98 | |
Mean | 14.021 | 11.613 | 47.929 | 63.188 |
SD | 0.915 | 0.579 | 3.870 | 5.002 |
SE | 0.236 | 0.149 | 0.999 | 1.292 |