Table 6.
Normality test and paired t-test analysis of rabbits implanted with polypropylene and ACTM after 48 weeks.
Pair | Kolmogorov-Smirnov | Shapiro-Wilk | Mean | SD | SE | 95% CI | t | P Value | ||||
---|---|---|---|---|---|---|---|---|---|---|---|---|
Statistic | df | Sig. | Statistic | df | Sig. | |||||||
Tensile stress (MPa): Polypropylene-ACTM | 0.194 | 15 | 0.133 | 0.889 | 15 | 0.066 | 2.319 | 0.486 | 0.125 | 2.050–2.588 | 18.497 | 3.093E−11 |
Tensile strain (%): Polypropylene-ACTM | 0.168 | 15 | 0.200 | 0.924 | 15 | 0.218 | −15.845 | 6.731 | 1.738 | −19.573–12.118 | −9.117 | 2.900E−07 |