Skip to main content
. 2020 Mar 11;5(11):5739–5747. doi: 10.1021/acsomega.9b03769

Table 5. Fresh Weight (FW) and Dry Weight (DW) of D. viscosa under CdO NPs Stressa.

  Cs-CdO NPs
As-CdO NPs
Ch-CdO NPs
conc. (mg/L) FW (mg) DW (mg) FW (mg) DW (mg) FW (mg) DW (mg)
0 139 ± 1.1d 50 ± 0.9d 139 ± 1.1d 50 ± 0.9c 139 ± 1.1c 50 ± 0.9c
2.5 184 ± 1.2b 83 ± 0.9b 192 ± 1.0a 90 ± 0.5a 163 ± 0.4b 70 ± 1.3b
5 199 ± 1.1a 95 ± 0.5a 142 ± 0.6c 48 ± 1.1c 123 ± 1.2d 44 ± 0.1d
10 151 ± 0.2c 60 ± 0.4c 163 ± 0.8b 66 ± 1.2b 188 ± 0.4a 90 ± 1.3a
20 117 ± 0.9e 24 ± 1.2e 123 ± 1.1e 40 ± 0.7d 110 ± 0.4e 33 ± 0.9e
a

Values represent mean ± standard error from triplicate. Different letters show a significant difference between them. As-CdO NPs (A. scoparia-synthesized), Cs-CdO NPs (C. sativa-synthesized), and Ch-CdO NPs (chemically synthesized CdO NPs).