Extended Data Fig. 5. Asymmetric grain boundary transformation at 600K.

Extended Data Fig. 5

a, Nucleation of a pearl GB phase at the open surface (left) of the asymmetric GB at 600K. b, Asymmetric pearl GB phase after the transformation at 600K is complete. The boundary remains asymmetric.