. 2016 Oct 20;202(2):217–235. doi: 10.1007/s10704-016-0157-z

Fig. 4.

Fig. 4

Non-zero components of the stress tensor of the microporous hydroxyapatite polycrystal according to Eqs. (4) and (9), for varying bone tissue volume fraction fbonecongl, and under physiologically relevant macroscopic stress according to Eq. (5), with Σcongl,11=-10MPa