Skip to main content
. 2020 Mar 11;7(3):191632. doi: 10.1098/rsos.191632

Figure 2.

Figure 2.

Powder X-ray diffraction pattern of Ga2Zr2−xWxO7 system calcined at 600°C/2 h (x = 0, 0.05, 0.1, 0.15 and 0.2).