Skip to main content
. 2020 Mar 13;13(6):1304. doi: 10.3390/ma13061304

Figure 6.

Figure 6

Figure 6

Fracture surface of M7B after SSRTT under different relative humidity (RH) conditions with different strain rates: (a,b) in air at 10−4 s−1; (c,d) in 60% RH at 10−5 s−1; (e,f) in 100% RH at 10−5 s−1; (gj) in 60% RH at 10−6 s−1; (k,l) in 100% RH at 10−6 s−1.