Skip to main content
. 2020 Mar 13;13(6):1304. doi: 10.3390/ma13061304

Figure 10.

Figure 10

Figure 10

Fracture surface of M10B after SSRTT under different RH conditions with different strain rates: (a,b) in air at 10−4 s−1; (c,d) in 60% RH at 10−4 s−1; (e,f) in 100% RH 10−4 s−1; (g,h) in 60% RH at 10−6 s−1; (i,j) in 100% RH at 10−6 s−1.