Skip to main content
. 2020 Mar 18;13(6):1371. doi: 10.3390/ma13061371

Figure 6.

Figure 6

Top: Foam densities of the neat PLA grades foamed after a 30 min. saturation with CO2 at 180 bar at varying temperatures. Bottom: SEM images of the foam with lowest density for each grade with crystallinity values (1st heating).